Investigation of Whisker Formation on Tin Plated Conductors

Standard:
Reaffirmed:
  • 2004-08-23
 
  • HISTORICAL Access the latest revision: AIR5444A
Publisher:
  • SAE International
Pages:
10
Scope:

This SAE Aerospace Information Report (AIR) shall be limited to general information about tin whisker formation on tin plated conductors. It summarizes the mechanisms of metal whisker formation and describes possible conclusions as related to tin plated conductors. It also provides a number of reference documents that describes research and observations of the whisker phenomena, recommendations to prevent its formation and conclusions.

The investigation by this task group of AE-8D was initiated by a request of the Naval Air Warfare Center, Indianapolis, Indiana, to determine if the phenomenon of tine whiskers is a problem in aerospace wire and cable.

This document provides some brief information about tin whisker formation and a list of reference documents that can provide more detailed information.

History:
Standard Published Revision Status
AIR5444A 2014-12-05 Latest Stabilized
2004-08-23 Historical Reaffirmed
AKA:
  • SAE AIR 5444
Sector:
Topic:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Book
2008-07-01