Plating, Chromium, Hard Deposit

Standard:
Revised:
  • 2015-01-07
 
  • CURRENT
Publisher:
  • SAE International
Pages:
7
Scope:

This specification covers the requirements for electrodeposited hard chromium plate.

Rationale:

AMS2406N changes the hydrogen embrittlement relief requirement to the standard wording of 40 HRC for use with AMS2759/9, added hydrogen embrittlement relief requirement for hardnesses of 36-39 HRC and changes adhestion testing from an acceptance test to a periodic test.

History:
Standard Published Revision Status
AMS2406N 2015-01-07 Latest Revised
2012-11-27 Historical Revised
2007-05-31 Historical Revised
2001-10-18 Historical Revised
2001-04-01 Historical Revised
1994-12-01 Historical Revised
1985-04-01 Historical Revised
1980-07-01 Historical Revised
1969-11-01 Historical Revised
1965-09-01 Historical Revised
1964-01-01 Historical Revised
1953-02-01 Historical Revised
1948-07-01 Historical Revised
1946-11-01 Historical Issued
AKA:
  • SAE AMS 2406
Sector:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Technical Paper / Journal Article
1956-01-01
Training / Education
2013-04-09
Training / Education
2013-04-09
Technical Paper / Journal Article
1952-01-01
Technical Paper / Journal Article
1958-01-01
Training / Education
2017-10-23