Heat Treatment of Carbon and Low-Alloy Steel Parts, Minimum Tensile Strength Below 220 ksi (1517 MPa)

Standard:
Reaffirmed:
  • 2014-04-23
Scope:

This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS2759.

Rationale:

AMS2759/1E has been reaffirmed to comply with the SAE five-year review policy.

History:
Standard Published Revision Status
AMS2759/1E 2014-04-23 Latest Reaffirmed
2007-06-13 Historical Revised
2000-09-01 Historical Revised
1996-12-01 Historical Revised
1996-09-01 Historical Revised
1994-04-01 Historical Revised
Buy
Select
Price
List
Download
$72.00
Add
Mail
$72.00
Members save up to 19% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2013-04-09
Training / Education
2013-04-09
Training / Education
2013-04-09
Technical Paper / Journal Article
2006-09-12
Technical Paper / Journal Article
2003-09-08
Standard
2004-12-29
Standard
2008-10-23
Article
2014-06-02
Training / Education
2013-04-09
Article
2014-05-31