Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher

Standard:
Reaffirmed:
  • 2014-04-23
 
  • CURRENT
Publisher:
  • SAE International
Pages:
13
Scope:

This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759.

Rationale:

AMS2759/2F has been reaffirmed to comply with the SAE five-year review policy.

History:
Standard Published Revision Status
AMS2759/2F 2014-04-23 Latest Reaffirmed
2011-08-10 Historical Reaffirmed
2009-07-20 Historical Revised
2007-08-24 Historical Revised
2000-09-01 Historical Revised
1996-12-01 Historical Revised
1996-09-01 Historical Revised
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2017-10-23
Training / Education
2013-04-09
Technical Paper / Journal Article
2008-09-16
Training / Education
2013-04-09
Technical Paper / Journal Article
2008-09-16
Training / Education
2013-02-20
Technical Paper / Journal Article
2011-04-12