Magnesium Alloy Castings, Sand, 4.0Y - 2.3Nd - 0.7Zr (WE43B - T6), Solution and Precipitation Heat Treated

Standard:
Revised:
  • 2007-06-13
 
  • HISTORICAL Access the latest revision: AMS4427C
Publisher:
  • SAE International
Pages:
8
Scope:

These castings have been used typically for parts requiring a combination of light weight, high yield strength up to 570 °F (298 °C), and relatively high corrosion resistance, but usage is not limited to such applications.

Rationale:

AMS 4427B is a Five Year Review and update of this specification.

History:
Standard Published Revision Status
AMS4427C 2012-06-01 Latest Revised
2007-06-13 Historical Revised
2001-11-19 Historical Revised
2000-09-01 Historical Reaffirmed
AKA:
  • SAE AMS 4427
Sector:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Technical Paper / Journal Article
1957-01-01
Technical Paper / Journal Article
1944-01-01
Technical Paper / Journal Article
1946-01-01
Technical Paper / Journal Article
1938-01-01
Article
2016-12-08
Technical Paper / Journal Article
1946-01-01
Technical Paper / Journal Article
1940-01-01