Steel, Corrosion and Heat Resistant, Investment Castings, 19Cr - 12Ni - 1.0(Cb + Ta), Solution Heat Treated

Standard:
Reaffirmed:
  • 2006-04-18
 
  • HISTORICAL Access the latest revision: AMS5362L
Publisher:
  • SAE International
Pages:
11
Scope:

This specification covers a corrosion and heat resistant steel in the form of investment castings.

These castings have been used typically for structural parts, where welding during fabrication may be required, for use up to 1500 degrees F (816 degrees C), but usage is not limited to such applications.

History:
Standard Published Revision Status
AMS5362L 2015-04-08 Latest Reaffirmed
2006-04-18 Historical Reaffirmed
2001-01-01 Historical Revised
1993-04-01 Historical Revised
1985-07-01 Historical Revised
1978-10-01 Historical Revised
1976-01-01 Historical Revised
1962-01-01 Historical Revised
1955-03-01 Historical Revised
1950-12-01 Historical Revised
1949-03-01 Historical Revised
1947-12-01 Historical Issued
AKA:
  • SAE AMS 5362
Sector:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2013-02-20
Technical Paper / Journal Article
2008-09-16
Training / Education
2017-10-23
Training / Education
2013-04-09
Technical Paper / Journal Article
2009-07-12
Training / Education
2013-04-09
Technical Paper / Journal Article
2014-04-20
Training / Education
2013-04-09