Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750°F (954°C) Solution Heat Treated

Standard:
Revised:
  • 2013-12-12
 
  • CURRENT
Publisher:
  • SAE International
Pages:
7
Scope:

This specification covers a corrosion and heat resistant nickel alloy in the form of sheet, strip, and plate.

These products have been used typically for parts requiring resistance to creep and stress-rupture up to 1300 degrees F (704 degrees C), oxidation resistance up to 1800 degrees F (982 degrees C), and good machinability, particularly for those parts which are formed or welded and then heat treated to develop required properties, but usage is not limited to such applications.

Rationale:

AMS5606F adjusts the size breaks for various properties (Tables 2, 3, 4, and 5) to more accurately reflect the breakpoint between sheet and plate, revises Bending (3.5.1.3), Stress Rupture Testing (3.5.2.3.2), Reports (4.4), and results from a Five Year Review and update of this specification.

History:
Standard Published Revision Status
AMS5606F 2013-12-12 Latest Revised
2006-03-10 Historical Revised
2000-09-01 Historical Revised
1992-01-01 Historical Revised
1986-07-01 Historical Revised
1979-07-01 Historical Revised
1971-11-01 Historical Issued
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2013-04-09
Article
2016-12-08
Training / Education
2013-04-09
Training / Education
2013-04-09