Steel, Corrosion Resistant, Bars, Wire, and Forgings 12cr 8.5ni 1.2ti 2.0cu Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable

Standard:
Revised:
  • 2000-09-01
 
  • HISTORICAL Access the latest revision: AMS5617J
Publisher:
  • SAE International
Pages:
11
Scope:

This specification covers two grades of a premium aircraft-quality, corrosion-resistant steel in the form of bars, wire, forgings, and forging stock.

These products have been used typically for parts requiring corrosion resistance and high strength up to 800F (425C). The steel can be precipitation hardened to minimum tensile strengths up to 225,000 psi (1550 Mpa).

Certain design and processing procedures may causes these products to become susceptible to stress-corrosion cracking after heat treatment; ARP 1110 recommends practices to minimize such conditions.

History:
Standard Published Revision Status
AMS5617J 2012-02-09 Latest Reaffirmed
2000-09-01 Historical Revised
1994-04-01 Historical Reaffirmed
1988-07-01 Historical Revised
1981-04-01 Historical Revised
1979-01-01 Historical Revised
1977-07-01 Historical Revised
1976-01-01 Historical Revised
1973-12-01 Historical Revised
1969-05-01 Historical Issued
AKA:
  • SAE AMS 5617
Sector:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2013-04-09
Training / Education
2013-04-09
Training / Education
2013-04-09
Training / Education
2017-10-23
Technical Paper / Journal Article
2008-09-16
Training / Education
2013-04-09
Technical Paper / Journal Article
2014-04-20