Steel, Corrosion and Heat-Resistant, Welding Wire 20Cr - 10Ni - 0.75Cb, High Ferrite Grade

Standard:
Revised:
  • 2014-02-27
 
  • CURRENT
Publisher:
  • SAE International
Pages:
5
Scope:

This specification covers a corrosion and heat resistant steel in the form of welding wire. This wire has been used typically as bare wire filler metal for gas-tungsten-arc or gas-metal-arc welding of corrosion and heat resistant alloys of similar composition, but usage is not limited to such applications.The relatively high ferrite content promotes weldability by combating microfissuring and minimizing cracking in heavy sections but limits use of the wire to applications not operating in the sigma-forming temperature range, approximately 1100 to 1600 degrees F (590 to 870 degrees C).

Rationale:

AMS5790D results from a Five Year Review and update to revise reference to the DeLong Diagram (2.3, 3.1.3) and Reports (4.4).

History:
Standard Published Revision Status
AMS5790D 2014-02-27 Latest Revised
2008-05-01 Historical Reaffirmed
1997-02-01 Historical Revised
1990-01-01 Historical Revised
1984-10-01 Historical Issued
AKA:
  • SAE AMS 5790
Sector:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2013-02-20
Training / Education
2013-04-09
Training / Education
2013-04-09
Training / Education
2011-04-09
Training / Education
2013-04-09
Article
2016-12-08