Steel Bars and Forgings 1.8ni 0.25mo (0.38-0.43c) (4640) Heat Treated, 125 Ksi (862 Mpa) Tensile Strength

Standard:
Revised:
  • 2003-01-22
 
  • HISTORICAL Access the latest revision: AMS6317K
Publisher:
  • SAE International
Pages:
8
Scope:

This specification covers an aircraft-quality, low-alloy steel in the form of heat treated bars and forgings.

These products have been used typically for parts with sections 1.0 inch (25 mm) and under in nominal thickness requiring a minimum tensile strength of 125 ksi (862 MPa), but usage is not limited to such applications.

History:
Standard Published Revision Status
AMS6317K 2017-08-24 Latest Revised
2012-11-05 Historical Revised
2007-10-16 Historical Revised
2003-01-22 Historical Revised
1995-05-01 Historical Reaffirmed
1986-01-01 Historical Revised
1978-10-16 Historical Revised
1971-11-15 Historical Revised
1945-07-01 Historical Revised
1942-03-01 Historical Revised
1939-12-04 Historical Issued
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Training / Education
2013-04-09
Training / Education
2013-04-09
Training / Education
2013-04-09
Training / Education
2017-10-23
Training / Education
2013-02-20
Training / Education
2013-04-09
Technical Paper / Journal Article
2013-10-07
Training / Education
2013-04-09