Bolts, Cobalt-Chromium-Nickel Alloy UNS R30159, Tensile Strength 260 ksi, Procurement Specification

Standard:
Revised:
  • 1997-03-01
 
  • HISTORICAL Access the latest revision: AS7475D
Pages:
26
Scope:

This procurement specification covers bolts made from a corrosion and heat resistant, work-strengthened, cobalt-chromium-nickel alloy of the type identified under the Unified Numbering System as UNS R30159. The following specification designations and their properties are covered: AS7475 260 ksi minimum ultimate tensile strength at room temperature; 205 ksi minimum ultimate tensile strength at 1100° F; 140 ksi stress-rupture strength at 1100° F; 135 ksi tension to 13.5 ksi tension fatigue at room temperature; AS7475-1 260 ksi minimum ultimate tensile strength at room temperature; 132 ksi miminum ultimate shear strength at room temperature.

History:
Standard Published Revision Status
AS7475D 2015-04-29 Latest Reaffirmed
2007-06-27 Historical Reaffirmed
2000-08-01 Historical Revised
1997-03-01 Historical Revised
1991-01-17 Historical Issued
AKA:
  • SAE AS 7475
Sector:
Access
Now
SAE MOBILUS Subscriber? You may already have access.
Buy
Select
Price
List
Download
$76.00
Add
Mail
$76.00
Members save up to 18% off list price.
Grade
If you are currently using this technical report:
Share
HTML for Linking to Page
Page URL

Related Items

Technical Paper / Journal Article
2014-04-20
Technical Paper / Journal Article
2009-11-10
Technical Paper / Journal Article
2008-04-14