Aluminum Coating, Ion Vapor Deposition

Scope:

This specification covers the engineering requirements for ion vapor deposition (IVD) of aluminum on steel, titanium, and aluminum alloys and the properties of the deposit.

This process has been used typically to provide a corrosion-resistant coating to parts operating at service temperatures up to 925 °F (496 °C) and requiring freedom from hydrogen embrittlement and solid metal embrittlement, but usage is not limited to such applications.