Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al- 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated

Scope:

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, 3.25 inches (82.6 mm) and under and stock of any size for forging and for flash welded rings. (see 8.5).

Rationale:

AMS5707M results from a limited scope ballot to revise Classification of Tests (4.2), Reports (4.4), and Identification (5.2.4).

Buy
WIP - Not available for purchase at this time.
Share
HTML for Linking to Page
Page URL

Related Items

Technical Paper / Journal Article
2004-09-21
Technical Paper / Journal Article
1999-10-06
Technical Paper / Journal Article
1999-10-06
Technical Paper / Journal Article
1999-10-06
Training / Education
2018-06-20
Technical Paper / Journal Article
1999-10-06